Adhesive
Loctite
EA E-40HT
DP420
DP460
Hysol E‐120HP
Tube and metal prep
Aluminum etching and Alodine coating to prevent corrosion and increase bond strength
West System 860 Aluminum Etching Kit
DuPont Acid Etch and Alodine solutions
Submerge Aluminum in etch solution, then submerge in non-diluted Alodine solution
Aluminum stock for insert
Check for appropriate lengths
Bond length increases linearly with bond strength
Gap 0.004 - 0.012 in for hot bonding
Gap 0.008 in for cold bonding
Carved aluminum, tapped for fitting a bearing insert
create shoulder only for grabbing in tensile test
In MIT paper, flashbreaker tape was used to add thickness at the end of the insert to create equal spacing and center insert.
Materials
x1 45552 CF Tuber (60in)
Produces x12 5-in test tubes
Process for Insert Tensile Test
...