Factors to consider

  • Core Material

    • Aluminum Honeycomb

    • Nomex Honeycomb

  • Face sheet materials

    • 4 ply either side, should we use Kevlar or Fiberglass for inner layer (galvanic)

    • In areas 500mm from driver, do we want to add more layers when adding the Kevlar or remove some layers

  • Adhesive

    • Co-bond using West Systems

    • Co-bond using Lam 127

    • Secondary bond using West Systems

    • Secondary bond using Lam 127

    • Secondary bond using Araldite

    • Secondary bond using paste epoxy

  • Filler materials

    • This would be for secondary bond epoxies, especially paste epoxies, in order to get ideal bond thickness (4-8 thou)

    • This has the potential to strengthen our panels but I have no data to back this up and it would have to be completely empirical

First test plans

  • No labels